Mild steel copper-coated oxy-acetylene gas welding rods are made of high-quality carbon steel of uniform and tightly controlled analysis. These rods have a melting point of 2750° F and produce quality welds of up to 65,000 PSI tensile strength. Ideal general purpose rod for welding all low-carbon steels.
Low-temperature, self-fluxing rod for use on aluminum and magnesium. 700° F melting temperature.
For use with bare bronze. Cleans well to allow for good adhesion. Comes in a 0.5 lb. canister.
Low-fuming bronze gas welding rods are made of copper/tin alloy to produce a rod that flows easily, joins a variety of metals including cast and malleable iron, galvanized steel, bronze, copper and steel. These rods have a melting point of 1630° F and produce strong joints up to 63,000 PSI tensile strength.
Low-fuming bronze gas welding rods are made of copper/tin alloy to produce a rod that flows easily, joins a variety of metals including cast and malleable iron, galvanized steel, bronze, copper and steel. These rods have a melting point of 1630° F and produce strong joints up to 63,000 PSI tensile strength.
Low-fuming bronze gas welding rods are made of copper/tin alloy to produce a rod that flows easily, joins a variety of metals including cast and malleable iron, galvanized steel, bronze, copper and steel. These rods have a melting point of 1630° F and produce strong joints up to 63,000 PSI tensile strength. Bare bronze rods require flux (see #770119).
Mild steel copper-coated oxy-acetylene gas welding rods are made of high-quality carbon steel of uniform and tightly controlled analysis. These rods have a melting point of 2750° F and produce quality welds of up to 65,000 PSI tensile strength. Ideal general purpose rod for welding all low-carbon steels.
Flat, high-strength, self-fluxing alloy for copper-to-copper (without flux) and copper-to-bronze with 5130 flux. Preheating is recommended for some applications.
Low-fuming bronze gas welding rods are made of copper/tin alloy to produce a rod that flows easily, joins a variety of metals including cast and malleable iron, galvanized steel, bronze, copper and steel. These rods have a melting point of 1630° F and produce strong joints up to 63,000 PSI tensile strength. Bare bronze rods require flux (see #770119).