Where to Buy
Service & Support
e-Learning
Weld Talk
Choose between AC or DC output to expand your welding options. The LX 235 AC/160 DC has a maximum of 235 AC and 160 DC weld output. Smooth DC weld performance with easy arc starts is easily adjusted with the Accu-Set® infinite amperage control. Weld time also increases up to 100% with decreased output, with the Accu-Set infinite amperage control.
| Comes complete with: |
|
||
|---|---|---|---|
| Power: |
|
||
| Processes: |
|
||
| Skill Level: | Moderate | ||
| Applications: |
|
| #043927 |
Running GearMounts easily to unit and provides convenient portability. Includes two wheels, two feet, and a handle. (Running gear is standard with #500419) |
|---|---|
|
Stick Electrodes View Electrode Chart |
| Stock Number | #500421 Standard | ||
|---|---|---|---|
| Rated Output at 25 VAC |
AC: 225 A at 20% Duty Cycle, 60 Hz 225 A at 15% Duty Cycle, 50 Hz |
||
|
DC: 150 A at 20% Duty Cycle, 60 Hz 150 A at 15% Duty Cycle, 50 Hz |
|||
| Max. Open-Circuit Voltage AC/DC | 80 V | ||
| Welding Amperage Ranges |
AC High: 40 - 235 A Low: 30 - 150 A |
||
| DC: 30 - 160 A | |||
| Amps Input at Rated Output, 60 Hz | 230 V: 47.5 | ||
| Dimensions | H: 18 3/4 in (476 mm) W: 12 3/4 in (323 mm) D: 17 1/2 in (445 mm) |
||
| Net Weight | 104 lb (47 kg) |
| Processes Recommended |
Steel | Stainless Steel |
Aluminum | Cast Iron | Copper | Brass | Titanium | Magnesium Alloys |
|---|---|---|---|---|---|---|---|---|
| Stick | X | X | X |