Hobart
Home » Products » Stick Electrodes & Welding Wire » Stick Electrodes
Bookmark and Share

Welding Electrodes

Excellent arc stability and reliable performance. Hobart stick electrodes are available in six industry-standard grades for a variety of applications. Available in 1, 5 and 10 lb. plastic reusable packs, or 50 lb. cartons. Each rod is printed with its AWS classification for easy identification and meets or exceeds all AWS specifications. Made in the U.S.A.

Get help choosing an electrode.

stick electrodes
stick Hobart electrode packaging is color coded for easy identification of electrode grade and has the electrode size prominently displayed when applicable.
line
6011 Welding Electrodes
An all-purpose stick electrode for use in all positions on carbon and galvanized steel. 60,000 PSI tensile strength. Deep penetrating, ideal for welding through light to medium amounts of dirty, rusty or painted materials. Runs on AC or DCEP (reverse) polarity.
Size 1 lb. Plastic 5 lb. Plastic 10 lb. Plastic 25 lb. Carton
1/16" #H112216-R01
3/32" #H112232-R01 #770456 #770458
1/8" #H112244-R01 #770459 #770460 #770457
5/32"
#770462 #770463 #770461
line
6013 Welding Electrodes
A light to medium penetrating all-purpose stick electrode for use in all positions, on carbon steel. Runs on AC or DCEP (reverse) polarity or DCEN (straight) polarity. 60,000 PSI tensile strength. Good for general, all-purpose applications and joints with poor fit-up.

Size Part No. Qty.    
1/16" #H117119-RDP
38
   
5/64" #H117125-RDP 23    
         
Size
1 lb. Plastic
5 lb. Plastic 10 lb. Plastic 25 lb. Carton
3/32" #H117132-R01 #770466 #770467
1/8" #H117144-R01 #770469 #770470 #770468
5/32"
#770472 #770473 #770471
line
7014 Welding Electrodes

For high-deposition requirements, this stick electrode is ideal for applications requiring light penetration and faster travel speeds. It runs in all positions on AC or DCEN (straight) or DCEP (reverse) polarity. 70,000 PSI tensile strength.

Size 1 lb. Plastic 5 lb. Plastic 10 lb. Plastic
1/16" #H114216-R01
3/32" #H114232-R01
1/8" #H114244-R01 #770464 #770465
5/32"
#770484 #770485
line
7018 Welding Electrodes

A low-hydrogen electrode for use in all positions on low, medium and high-carbon steels.
70,000 PSI tensile strength. Ideal for out-of-position welding and tacking. Runs on AC or
DCEP (reverse) polarity. Not recommended for low-voltage AC welders.

Size 1 lb. Plastic 5 lb. Plastic 10 lb. Plastic 25 lb. Carton
1/16" #H119916-R01
3/32" #H119932-R01 #770482 #770476
1/8" #H119944-R01 #770478 #770479
#770477
5/32"
#770480 #770481
line
7018AC Welding Electrodes

Same as above, but specially formulated to operate with small 208/230 volt AC welders.

Size 1 lb. Plastic 5 lb. Plastic 10 lb. Plastic
3/32" #H119832-R01
1/8" #H119844-R01 #770474 #770475