Gas Welding Rods
Mild steel copper-coated oxy-acetylene gas welding rods are made of high-quality carbon steel of uniform and tightly controlled analysis. These rods have a melting point of 2750° F and produce quality welds of up to 65,000 PSI tensile strength. Ideal general purpose rod for welding all low-carbon steels. Available in 1 lb. packs.

Part No. Type Diameter Length Qty.
#770514 Copper-Coated Steel (RG-45) 3/32" 18" 8
#770513 Copper-Coated Steel (RG-45) 1/8" 18" 8

Low-fuming bronze gas welding rods are made of copper/tin alloy to produce a rod that flows easily, joins a variety of metals including cast and malleable iron, galvanized steel, bronze, copper and steel. These rods have a melting point of 1630° F and produce strong joints up to 63,000 PSI tensile strength. Bare bronze rods require flux (see #770119 below). Available in 1 lb. packs.

Part No. Type Diameter Length Qty.
#770510 Bare Bronze 3/32" 18" 8
#770509 Bare Bronze 1/8" 18" 8
#770512 Flux-Coated Bronze 3/32" 18" 8
#770511 Flux-Coated Bronze 1/8" 18" 8
Gas Welding Rods
line
Brazing Rods (Uncoated)
Flat, high-strength, self-fluxing alloy for copper-to-copper (without flux) and copper-to-bronze with 5130 flux. Preheating is recommended for some applications.

Part No. Diameter Length Qty.
#770205 1/8" 17-1/2" 10

rods
line
Aluminum Rods
Low-temperature, self-fluxing rod for use on aluminum and magnesium. 700° F melting temperature.

Part No. Diameter Length Qty.
#770206 XX" 18-1/8" 8

line
Brazing Flux
For use with bare bronze. Cleans well to allow for good adhesion. Comes in a 0.5 lb. canister. #770119